Zirconia corundum brick Casting methods
Items | Zirconia corundum brick 33 | Zirconia corundum brick 36 | Zirconia corundum brick 41 | ||
Chemical components | Al203 | Leavings | Leavings | Leavings | |
ZrO2 | 32-36% | 35-40% | 40-44% | ||
SiO2 | 16.00% | 14.00% | 13.00% | ||
Na2O | 1.45% | 1.45% | 1.30% | ||
Fe2O3+TiO2+CaO+MgO+K2O | 0.55% | 0.55% | 0.55% | ||
FeO+TiO | 0.30% | 0.30% | 0.30% | ||
Buck density | 3.75 | 3.8 | 3.95 | ||
Apparent porosity | 1.50% | 1% | 1% | ||
Anti-erosion speed of glass liquid under static state (normal soda-lime glass, 1500℃×36h) | 1.6 | 1.5 | 1.3 | ||
Glass phase primary temperature | 1400℃ | 1400℃ | 1400℃ | ||
Bubble exhalation rate (normal soda-lime glass, 1300℃×10h) | 2.00% | 1.50% | 1% | ||
Glass phase exudation (1500℃×4h) | 2.00% | 3.00% | 3.00% | ||
Bulk Density | PT/QX | 3.45 | 3.45 | 3.55 | |
ZWS | 3.6 | 3.7 | 3.85 | ||
WS | 3.7 | 3.8 | 3.95 |